Most Venetian plastering problems, such as hairline cracks, dull patches, uneven sheen and joint lines showing through, trace back to the wall underneath or to the order in which the coats were laid, not to the plaster itself. Zavoré installs Venetian plaster across the UK, and almost every fault below can be avoided with a proper survey, the right preparation and a finish chosen for how the room is used.
Our Venetian plaster installation page shows how we run a job to avoid them, and our page on Venetian plastering across the UK lists the places we cover. Here we go through the common problems one by one, what usually causes them and how to stop them happening.
Fine cracks are the problem people ask about most. The plaster itself is seldom where the trouble starts. Cracks tend to follow something in the wall behind it. On plasterboard, an unreinforced joint is the classic culprit, because the line where two boards meet is a weak point. On older walls, cracks often follow an earlier repair, a change of material such as brick meeting timber, or a structural crack that was filled and painted over years ago.
The way to avoid it is preparation. Plasterboard joints are reinforced and the right primer is applied before any coat goes on. On solid walls, loose or hollow plaster is cut out and made good, and existing cracks are investigated rather than hidden. If a wall shows signs of ongoing movement, that needs a builder or surveyor first, not a decorative finish.
A polished finish shows every dip, so a wall that is wavy along its length will catch the light unevenly however well the plaster is laid. That is why flat walls matter so much, and why uneven walls are skimmed before a high polish. Dull patches can also appear where the burnishing has not been carried out evenly across the whole wall, or where a wax has been applied thinly in some places and heavily in others.
Planning helps here too. When a wall is laid in one continuous session by the same artisans, each coat goes on and is burnished in order, without stops and starts that can leave visible differences. That is one reason we plan work in blocks of days rather than calling in for an hour here and there.
When a pattern of lines or squares shows faintly through a finished wall, it usually mirrors the board joints, screw heads or filler underneath. Filler that has shrunk or a joint that was not reinforced can telegraph through thin coats. The fix is the same as for cracks, good preparation and the correct primer, so the base is even in both flatness and absorbency before the first coat.
Damp is not something a decorative finish can cure. Lime breathes, which helps an older solid wall stay healthy, but if water is getting in from outside or rising from below, the cause has to be found and fixed before plastering. Otherwise the problem can show through the finish later. The survey looks for damp, and if a wall needs repair first, we will say so plainly.
It can if the sample was never seen in the room. Colour shifts between daylight and lamps, and between a small chip and a whole wall. We tint every batch to the approved sample, from 48 house colours or any NCS reference. Look at a sample board in the room in the morning and again in the evening before you approve it, and you will rarely be surprised.
Lime is caustic while wet, so floors, joinery and skin are protected during the work. Read more about the material itself on our page about real lime Venetian plaster.
Often, yes. Small areas can be cut back and refinished, though blending the sheen and colour takes care. If the crack comes from movement in the wall, that cause has to be dealt with first, or the repair will simply crack again.
Each has its place. Lime breathes and suits solid masonry, while acrylic forms a film. Either way, the base and its preparation matter far more than the type of plaster, which is why the survey comes first.
Uneven wax is a common reason. A wall waxed heavily in some places and lightly in others will reflect light unevenly. Burnishing it evenly, and following the right aftercare, usually settles the surface.
They can if the joints are not reinforced or the wrong primer is used. Done properly, plasterboard takes Venetian plaster well, and it is one of the most common bases in new builds and flats.
If you are planning a wall or worried about an existing one, call +44 7592 929191 from Monday to Saturday, 9am to 6pm, or email photos, rough measurements and the address to sales@zavore.co.uk and we will talk it through.
How painting companies in Dubai can order Lime Paint for villa repaint work, with colours tinted room by room, labelled tubs and tracked ...
ContractorsHow plastering contractors can add microcement, tadelakt, limewash and Venetian plaster through Zavoré 1 to 1 Training, group courses of ...
Abu DhabiIf you searched for Venetian plaster paint for a villa in the UAE, here is what we actually supply, which real plaster to order instead a...
CoursesWhat three days on the Zavoré tadelakt course involve, from the base and radiused corners to the burnishing window, the stone, the soap a...
CoursesAn honest look at general plastering courses against the Zavoré Beginner Course in Venetian plaster at our Manchester centre, who each su...
Abu DhabiWhere Venetian plaster belongs in an Abu Dhabi villa bathroom, which finish takes over in the wet zone, and how the walls are sealed, sur...
Providing luxury finishes for the most prestigious addresses in the world
Venetian plaster, limewash, microcement, tadelakt, metallics, sculptural plaster and gold leaf, supplied and installed by our own team, with Venetian plaster taught at our Birmingham studio.
One list, run by the people who make the material. No noise, and nothing we would not want to read ourselves.
We email as the house has something worth saying, never daily. Unsubscribe from any email, or reply STOP to any text. We never pass your details to anyone.